Klinke, A., Gok, A., Ifeanyi, S., & Bruckman, L.(2018).A non-destructive method for crack quantification in photovoltaic backsheets under accelerated and real-world exposures.Polymer Degradation and Stability,153, 244-254.
Braid, J., Curran, A., Sun, J., Schneller, E., Fada, J., Liu, J., Wang, M., Longacre, A., Dai, J., Huey, B., Davis, K., Jaubert, J., & Bruckman, L.(2018).EL and I-V Correlation for Degradation of PERC vs. Al-BSF Commercial Modules in Accelerated Exposures..
\customboldJ. L. Braid, Curran, A., Sun, J., Schneller, E., Fada, J., Liu, J., Wang, M., Longacre, A., Dai, J., Huey, B., Davis, K., Jaubert, J., & Bruckman, L.(2018).EL and I-V Correlation for Degradation of PERC vs. Al-BSF Commercial Modules in Accelerated Exposures..
Wang, Y., Huang, W., Fairbrother, A., Loyer, C., Hauser, A., Julien, S., Gu, X., O'Brien, G., Boyce, K., Kempe, M., Wan, K., & Bruckman, L.(2018).Accelerated Exposure Tests for Photovoltaic Backsheets to Cross-Correlate Real-World Climate Zones..
Miller, D., Annigoni, E., Ballion, A., Bokria, J., Bruckman, L., Burns, D., Chen, X., Feng, J., Fowler, S., Honeker, C., Kempe, M., Khonkar, H., Köhl, M., Perret-Aebi, L., Phillips, N., Scott, K., Sculati-Meillaud, F., & Wohlgemuth, J.(2018).Degradation in PV encapsulant strength of attachment: An interlaboratory study towards a climate-specific test..
Jalabert, D., Zaid, H., Berger, M., Fongkaew, I., Lambrecht, W., & Sehirlioglu, A.(2018).Ion blocking dip shape analysis around a LaAlO 3 /SrTiO 3 interface.Nuclear Instruments and Methods in Physics Research, Section B: Beam Interactions with Materials and Atoms,423, 67-71.
Zaid, H., Berger, M., Jalabert, D., Walls, M., Akrobetu, R., Goble, N., Gao, X., Berger, P., Fongkaew, I., Lambrecht, W., & Sehirlioglu, A.(2018).Role of the different defects, their population and distribution in the LaAlO 3 /SrTiO 3 heterostructure's behavior.Journal of Applied Physics,123(15).
Klinke, A., Gok, A., Ifeanyi, S., & Bruckman, L.(2018).An Automated Algorithm for Quantifying Cracks in Photovoltaic Backsheets Under Accelerated and Real-World Exposures.IEEE.
Gordon, D., Huang, W., Burns, D., French, R. H., & Bruckman, L. H.(2018).Multivariate multiple regression models of poly(ethylene-terephthalate) film degradation under outdoor and multi-stressor accelerated weathering exposures.PLOS ONE,13(12).
Braid, J., Curran, A., Sun, J., Schneller, E., Fada, J., Liu, J., Wang, M., Longacre, A., Dai, J., Huey, B., Davis, K., Jaubert, J., & Bruckman, L.(2018).EL and I - V Correlation for Degradation of PERC vs. Al-BSF Commercial Modules in Accelerated Exposures.IEEE.
Verma, A., French, R. H., & Carter, J. W.(2017).Physics Informed Network Models: Data Science Approach to Metals Design.Integrating Materials and Manufacturing Innovation/Springer,6(4),279–287.
Fairbrother, A., Avenet, J., Lyu, Y., Boyd, M., Julien, S., Wang, K., Ji, L., Boyce, K., Merzlic, S., Lefebvre, A., O'Brien, G., Wang, Y., Bruckman, L., Kempe, M., Dougherty, B., & Gu, X.(2017).Photovoltaic Array Differential Backside Exposure Conditions: Backsheet Degradation and Site Design..
Wang, Y., Merzlic, S., Fairbrother, A., Julien, S., Fridman, L., Loyer, C., Lefebvre, A., O'Brien, G., Gu, X., Ji, L., Boyce, K., Kempe, M., Wang, K., & Bruckman, L.(2017).Degradation Models of Photovoltaic Module Backsheets Exposed to Diverse Real World Condition..
Gok, A., Ngendahimana, D., Fagerholm, C., French, R. H., Sun, J. H., & Bruckman, L. H.(2017).Predictive models of poly(ethyleneterephthalate) film degradation under multifactor accelerated weathering exposures.PLoS ONE,12(5).
Fairbrother, A., Julien, S., Wan, K., Ji, L., Boyce, K., Merzlic, S., Lefebvre, A., O'Brien, G., Wang, Y., Bruckman, L., & Others, L.(2017).Degradation analysis of field-exposed photovoltaic modules with non-fluoropolymer-based backsheets.,10370, 1037003.
Wang, Y., Fairbrother, A., Merzlic, S., Julien, S., Fridman, L., Loyer, C., Lefebvre, A., O'Brien, G., Gu, X., Ji, L., Boyce, K., Kempe, M., Wan, K., & Bruckman, L.(2017).Model development of degradation of PV modules backsheet with locating place of module.,10370
Kowalski, B., & Sehirlioglu, A.(2017).High temperature limitation due to onset of depoling in BiScO 3 PbTiO 3.Journal of Applied Physics,121(6),064106.
Matthews, R., Glasser, E., Sprawls, S., French, R. H., Peshek, T. H., Pentzer, E. H., & Martin, I. H.(2017).Organofunctional Silane Modification of Aluminum-Doped Zinc Oxide Surfaces as a Route to Stabilization.ACS Applied Materials & Interfaces,9(20),17620-17628.
Gordon, D., Denoyer, L., Meyer, C., Sweet, N., Burns, D., & Bruckman, L.(2017).Characterizing the Weathering Induced Changesin Optical Performance and Properties of Poly(ethylene-terephthalate) via MaPd:RTS Spectroscopy.SPIE-INT SOC OPTICAL ENGINEERING,10370
Klinke, A., Gok, A., Ifeanyi, S., & Bruckman, L.(2017).Degradation of photovoltaic backsheet materials under multi-factor accelerated UV light exposures.,10370, 1037004.